"Practically, a sufficient flow range in a premixed paste is a proof of the effective production of FC. When the value of flow seen was lesser than the limit, the mixes of the developed premixed paste and foam was considered in-cohesive. The binders seemed to be covered by air bubbles, which collapsed afterwards. [W]hen the value of flow was greater than the limit, seclusion happened and foam bubbles inclined to collapse."
Quote Details
Added by wikiquote-import-bot
Unverified quote
0 likes
Original Language: English
Available Languages (1)
Sources
Imported from EN Wikiquote
https://en.wikiquote.org/wiki/Foam_concrete
Revision History
No revisions have been submitted for this quote.
Categories
Foam concrete
176 quotes on TrueQuotesView all quotes by Foam concrete →
Related Quotes
"[L]ower water content leads to a hard mixture... easily resulting in bubble bursting..."
"The (ACI) recommends that mixed water should be fresh, clean, and drinkable..."
"Over the past 30 years, FC are widely used for the bulk filling... ditch repair, retaining wall...bridge backfill... …"
"The water requirement for constituent material depends on composition, consistency and stability of the mortar body..."
"FC was initially envisaged as a void filling, stabilization, and insulation material..."
"[H]igher water content causes mixture too thin to accommodate bubbles... causing bubbles separating from the mixture..."
"This CPAR project was undertaken to test, demonstrate, and commercialize a new construction system... [which] employs…"
"The booming development of this new constituent material in buildings and constructions was enhanced in the late 1970…"
"The basic components of FC consist of (1) water, (2) binder, (3) foaming agent, (4) filler, (5) additive, and (6) fiber."
"Cement is the most commonly used binder. The ordinary , rapid hardening Portland cement, calcium sulphoaluminate ceme…"