"The mortar used for the hulls was a mixture of clean, graded silica sand, ...Portland Cement Type II, and drinking-type water. This silica sand, of the grading and particle shape used in high-strength structures... The sand content used was... one 50-pound (22 Kg) bag of coarse grade, one 100-pound (44 Kg) bag of medium grade and one 50-pound (22 Kg) bag of fine grade. To this graded sand was added two 80-pound (31 Kg) bags of Portland Cement Type II and just sufficient water to make the mortar workable into the hull mesh reinforcing. ...There was one plasterer for roughly every 100 square feet (9 m2) ...Retarders or additives were not used. The sun shelters were moved into place ..."